Title: | Восстановительное дебромирование бромсодержащих фенолов |
Authors: | Балабанович, А. И. Прокопович, В. П. |
Keywords: | ЭБ БГУ::ЕСТЕСТВЕННЫЕ И ТОЧНЫЕ НАУКИ::Химия |
Issue Date: | Feb-2008 |
Publisher: | БГУ |
Citation: | Вестник Белорусского государственного университета. Сер. 2, Химия. Биология. География. – 2008. - №1. – С. 32-37. |
Abstract: | They can be debrominated to phenol, alkylphenols and HBr using polypropylene (PP), poly(vinyl alcohol) (PVA) or poly(vinyl amine) (PVAm) as reductive media. Relevant pyrolysis experiments have been carried out with Tetrabromobisphenol A in encapsulated ampoules. The temperature required for the reductive debromination reaction has been found to depend on the polymer media and decreases in the series PP (340 °C) – PVA (300 °C) – PVAm (240 °C). The reaction mechanism has been discussed in terms of radical hydrodebromination. = Показана возможность дебромирования бромсодержащик фенолов до фенола, алкилфенолов и бромистого водорода в среде полипропилена (ПП), поливинилового спирта (ПВС) и поливиниламина (ПАМ) на примере пиролиза тетрабромбисфенола А, проведенного в капсулированных ампулах. Найдено, что температура реакции восстановительного дебромирования зависит от полимерной среды и уменьшается в ряду ПП (340 °C) – ПВС (300 °C) – ПАМ (240 °C). Обсуждается радикальный механизм реакции. |
URI: | http://elib.bsu.by/handle/123456789/5582 |
ISSN: | 0372-5340 |
Licence: | info:eu-repo/semantics/openAccess |
Appears in Collections: | 2008, №1 (февраль) |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
pages 32-37 from Вестник_БГУ_Февраль_2008_Серия2_№1.pdf | 692,6 kB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.