https://elib.bsu.by/handle/123456789/340501| Title: | Влияние архитектуры подслоев на основе поликарбоната и серной кислоты на морфологию углеродных покрытий |
| Other Titles: | Influence of Architecture of Sublayers Based on Polycarbonate and Sulfuric Acid on the Morphology of Carbon Coatings / Rudenkov A. |
| Authors: | Руденков, А. С. |
| Keywords: | ЭБ БГУ::ЕСТЕСТВЕННЫЕ И ТОЧНЫЕ НАУКИ::Физика |
| Issue Date: | 2025 |
| Publisher: | Минск : БГУ |
| Citation: | Взаимодействие излучений с твердым телом : материалы 16-й Междунар. конф., Минск, Беларусь, 22-25 сент. 2025 г. / Белорус. гос. ун-т ; редкол.: В. В. Углов (гл. ред.) [и др.]. – Минск : БГУ, 2025. – С. 510-513. |
| Abstract: | Предложена оригинальная двухстадийная методика формирования трехслойных покрытий, заключающаяся в предварительном осаждении слоев на основе поликарбоната и серной кислоты путем электронно-лучевого диспергирования исходных компонентов и последующем нанесении углеродных слоев из плазмы импульсного катодно-дугового разряда. Показано, что порядок следования слоев поликарбоната и серной кислоты определяет морфологические особенности всего подслоя. Средствами атомно-силовой микроскопии установлено, что двухслойные системы поликарбонат/серная кислота характеризуются меньшей шероховатостью (9 нм), но более высокими значениями продольных размеров отдельных структурных образований (до 630 нм), по сравнению с покрытиями с архитектурой серная кислота/поликарбонат. В то же время углеродные покрытия, осажденные на подслое с архитектурой поликарбонат/серная кислота характеризуются более высокими значениями шероховатости (158 нм), чем слои, сформированные на подслое серная кислота/поликарбонат. Термообработка покрытий при температуре 120 °С в течение 30 мин на воздухе существенным образом влияет на морфологию рассматриваемых образцов. Углеродные слои, сформированные на поверхности поликарбонат/серная кислота после термообработки, характеризуются меньшими значениями среднего диаметра зерен (870 нм) и меньшей субшероховатостью (96 нм), чем слои, сформированные на этих же системах без термообработки |
| Abstract (in another language): | An original two-stage technique for forming three-layer coatings is proposed. It consists of preliminary deposition of layers based on polycarbonate and sulfuric acid by electron-beam dispersion of the initial components and subsequent application of carbon layers from the plasma of a pulsed cathode-arc discharge. It is shown that the order of the polycarbonate and sulfuric acid layers determines the morphological features of the entire sublayer. Atomic force microscopy has shown that the two-layer systems polycarbonate/sulfuric acid are characterized by lower roughness (9 nm), but higher values of the longitudinal dimensions of individual structural formations (630 nm), compared to coatings with the sulfuric acid/polycarbonate architecture. At the same time, carbon coatings deposited on the sublayer with the polycarbonate/sulfuric acid architecture are characterized by higher roughness values (158 nm) than the layers formed on the sulfuric acid/polycarbonate sublayer. Heat treatment of the coatings at a temperature of 120 °С for 30 minutes in air significantly affects the morphology of the samples under consideration. Carbon layers formed on the surface of polycarbonate/sulfuric acid after heat treatment are characterized by smaller values of the average grain diameter (870 nm) and lower sub-roughness (96 nm) than the layers formed on the same systems without heat treatment. Carbon layers formed on sulfuric acid/polycarbonate systems are characterized by a larger grain diameter (1610 nm), higher sub-roughness values (154 nm) than in the case of forming carbon coatings without preliminary heat treatment of the sublayer. The use of two-layer systems based on polycarbonate and sulfuric acid allows controlling the morphological features of the carbon layers deposited on their surface, which in turn is due to the processes of phase transformation of polycarbonate due to heat treatment and interaction with sulfuric acid |
| Description: | Секция 5. Методы, оборудование, плазменные и радиационные технологии = Section 5. Methods, Equipment, Plasma and Radiation Technologies |
| URI: | https://elib.bsu.by/handle/123456789/340501 |
| ISSN: | 2663-9939 (print) 2706-9060 (online) |
| Sponsorship: | Работа выполнена при финансовой поддержке Министерства образования Республики Беларусь в рамках комплексного задания 1.12, ГПНИ «Фотоника и электроника для инновации». |
| Licence: | info:eu-repo/semantics/openAccess |
| Appears in Collections: | 2025. Взаимодействие излучений с твердым телом |
Files in This Item:
| File | Description | Size | Format | |
|---|---|---|---|---|
| 510-513.pdf | 142,82 kB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.