Заглавие документа: Annealing Effect on Structural, Optical and Electrophysical Properties of ZnSe Nanocrystals Synthesized into SiO2/Si Ion Track Template
Авторы: Akylbekova, Aiman
Dauletbekova, Alma
Baimukhanov, Zein
Vlasukova, Liudmila A.
Usseinov, Abay
Saduova, Nuray
Akilbekov, Abdirash T.
Pankratov, Vladimir A.
Popov, Anatoli I.
Тема: ЭБ БГУ::ЕСТЕСТВЕННЫЕ И ТОЧНЫЕ НАУКИ::Физика
ЭБ БГУ::ЕСТЕСТВЕННЫЕ И ТОЧНЫЕ НАУКИ::Химия
Дата публикации: 22-авг-2024
Библиографическое описание источника: Aiman Akylbekova, Dauletbekova A, Zein Baimukhanov, Vlasukova LA, Abay Usseinov, Nuray Saduova, et al. Annealing Effect on Structural, Optical and Electrophysical Properties of ZnSe Nanocrystals Synthesized into SiO2/Si Ion Track Template. Materials. 2024 Aug 22;17(16):4149–9.
Аннотация: We report the results of synthesis of zinc selenide (ZnSe) nanocrystals into SiO2/Si track templates formed by irradiation with 200 MeV Xe ions up to a fluence of 107 ions/cm2 . Zinc selenide nanocrystals were obtained by chemical deposition from the alkaline aqueous solution. Scanning electron microscopy, X-ray diffractometry, Raman and photoluminescence spectroscopy, and electrical measurements were used for characterization of synthesized ZnSe/SiO2nanoporous/Si nanocomposites. XRD data for as-deposited precipitates revealed the formation of ZnSe nanocrystals with cubic crystal structure, spatial syngony F-43m (216). According to non-empirical calculations using GGA-PBE and HSE06 functionals, ZnSe crystal is a direct-zone crystal with a minimum bandgap width of 2.36 eV and anisotropic electronic distribution. It was found that a thermal treatment of synthesized nanocomposites at 800 ◦C results in an increase in ZnSe nanocrystallites size as well as an increase in emission intensity of created precipitates in a broad UV-VIS spectra range. However, vacuum conditions of annealing still do not completely prevent the oxidation of zinc selenide, and a formation of hexagonal ZnO phase is registered in the annealed samples. The current–voltage characteristics of the synthesized nanocomposites proved to have n-type conductivity, as well as increased conductivity after annealing.
URI документа: https://elib.bsu.by/handle/123456789/323045
DOI документа: 10.3390/ma17164149
Лицензия: info:eu-repo/semantics/openAccess
Располагается в коллекциях:Статьи

Полный текст документа:
Файл Описание РазмерФормат 
materials-17-04149.pdf3,51 MBAdobe PDFОткрыть
Показать полное описание документа Статистика Google Scholar



Все документы в Электронной библиотеке защищены авторским правом, все права сохранены.